Molybdenum Alloy Rods
Material Composition Molybdenum alloy (typically with additives) Density 9.6-10.2g/cm³ Melting Point Approximately 2,620 degrees Celsius (4,748 degrees Fahrenheit) Thermal Conductivity 138 – 142 W/m·K Coefficient of Expansion 4.8 – 5.2 x 10^(-6) K^(-1) Electrical Conductivity 30 – 35% IACS (International Annealed Copper Standard) Elastic Modulus 320 – 350 GPa Hardness (Mohs) 5.5 Tensile Strength 700 – 1,000 MPa Yield Strength 400 – 800 MPa Elongation at Break 10 – 20%